Home > Products > Casting Polyurethane Prepolymer > CPU For Elastomers > Polyester Polyol and Toluene Diisocyanate Prepolymer

Polyester Polyol and Toluene Diisocyanate Prepolymer

  • Product Description
Overview
Product Attributes

Model No.XCPU-E843S

BrandXuchuan Chemical

Place Of OriginChina

Types OfSynthetic Resin And Plastics

Name Of ProductsXCPU-E843S

Appearancessolid

Featuresexcellent wear resistance, oil resistance, mechanical properties

UsesSieve, machinery parts, sealing ring, PU roller and other products

BrandXuchuan

Supply Ability & Additional Information

Packaging20 & 200 kg/drum

Productivity250000MT/year

TransportationOcean

Place of OriginChina

Supply Ability250000 tons/year

HS Code39095000

PortShanghai

Payment TypeL/C,T/T,D/P

IncotermFOB,CFR,CIF

Packaging & Delivery
Selling Units:
Kilogram
Package Type:
20 & 200 kg/drum
Picture Example:


Product Description

Cpu For Elastomers


Polyester Polyol and Toluene Diisocyanate Prepolymer

Polyether Polyurethane Prepolymer

POLYSETER PREPOLYMER  XCPU-E843S

1,This product is a polyester polyol and toluene diisocyanate (T-80) in the

 synthesis of polyester polyurethane prepolymer

2,Features: excellent wear resistance, oil resistance, mechanical properties

3,Uses: Sieve, machinery parts, sealing ring, PU roller and other products

4,Typical propertties of PU matrix:

Name of products

Appearances

Viscosity(mPa.s/85)

NCO% content

Package(kg)

XCPU-E843S

solid

2000-2200

4.30-4.50

20 / 200

5,Operating procedures:

Prepolymer at 80 ~ 85  preheating, after vacuum degassing, the melt TMP 

good homogeneous mixing, deaeration, pouring, molding, vulcanization molding, 

stripping, vulcanization.

6,Reactioon parameter and physical properties:


Article Number

XCPU-E843S

Prepolymer/ g

100

100

100

100

100

Plasticizer /g

0

20

40

50

60

TMP/g

4.3

4.3

4.3

4.3

4.3

Pot Life (adjustable)

0.5~2h

Post Cure Time /(h/℃)

16/100

16/100

16/100

16/100

16/100

Temperature/℃(Prepolymer /TMP)

90/90

90/90

90/90

90/90

90/90

Hardness(Shore A)

60

50

40

35

30

Tensile Strength /MPa

20

15

6

5

3

Elongation / %

500~600

Angle Tear Strength, Die C /(KN/m)

25

20

15

13

10

Resilience (25)/ %

20

40

58

60

60

Gravity (25℃)/(g/ cm3)

1.22~1.27

Polyseter Prepolymer For Ring


Company Information

 

Product Categories : Casting Polyurethane Prepolymer > CPU For Elastomers

Home > Products > Casting Polyurethane Prepolymer > CPU For Elastomers > Polyester Polyol and Toluene Diisocyanate Prepolymer
Email to this supplier
  • *Subject:
  • *To:
    Mr. Javan
  • *Email:
  • *Message:
    Your message must be between 20-8000 characters
Send Inquiry
*
*

Home

Product

Whatsapp

About Us

Inquiry

We will contact you immediately

Fill in more information so that we can get in touch with you faster

Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.

Send